The most commonly used putty powder is hydroxypropyl methylcellulose (HPMC), Advantages of HPMC: strong water retention, stable thickening effect, good alkali resistance (suitable for cement-based putty), moderate film-forming properties, balancing workability and curing performance, making it the mainstream choice.
 Water Retention and Thickening to Prevent Rapid Drying
 
After application, putty needs to adhere tightly to the substrate (wall), and the cementitious materials (such as cement and gypsum) require water to complete the hydration reaction. The hydrophilic groups (hydroxyl groups, ether bonds) in the cellulose molecular chain can adsorb a large amount of water, forming a "moisture protective film," slowing down the penetration of water into the substrate (such as dry walls) and the rate of evaporation into the air, preventing the putty from cracking, blistering, and powdering due to rapid drying.

Simultaneously, cellulose forms a three-dimensional network structure in water, increasing the viscosity (consistency) of the putty slurry, preventing "sagging" during construction (especially on vertical surfaces) due to excessive thinness.

 Improved Workability (Workability, Plasticity)

Cellulose imparts good "thixotropic properties" to the putty: when standing, the slurry has a high consistency (not easily sedimenting or separating); during construction, mixing, or application (under shear force), the consistency decreases (easy to spread); after application, the shear force disappears, and the slurry quickly recovers its consistency, ensuring a uniform putty layer thickness and reducing "stickiness" or "collapse." For putty applied by hand scraping or machine spraying, suitable cellulose can make the putty easier to apply and smooth on the wall, reducing scraper resistance and improving construction efficiency.

 Enhanced Bond Strength and Crack Resistance

During the putty hardening process, cellulose molecular chains form a thin film, filling the gaps between filler particles and enhancing the "bridging effect" within the putty. This improves the adhesion between the putty layer and the substrate (reducing peeling), while also reducing the shrinkage rate of the hardened putty, minimizing micro-cracks.

For gypsum-based putty, cellulose can also alleviate the volume expansion caused by excessively rapid hydration of gypsum, preventing cracking.

 Stabilizes the system and prevents stratification and sedimentation

After the putty powder is mixed with water, the thickening effect of cellulose stabilizes the suspended state of solid particles (heavy calcium carbonate, cement, etc.) in the paste, preventing the "thin on top, thick on bottom" or filler sedimentation that occurs during standing. This ensures uniform putty composition and a smooth surface after application.
 
HEMC And HPMC Comparison.jpg

Compare HEMC vs HPMC through gelation temperature, water retention, and tile adhesive open time. Learn why grade chemistry and test methods matter, avoid misleading performance assumptions, and use a practical evaluation workflow to select cellulose ethers for demanding dry-mix mortar applications.

11 October 2026
HEC Hydration And Application Testing.jpg

Explore five HEC sourcing options for Indonesia, comparing manufacturers and distributors, disclosed capacity, MOQ transparency, and certification checks. Learn how to assess viscosity, hydration, samples, OEM support, and import logistics before selecting a long-term cellulose ether partner with care.

10 October 2026
Controlled HPMC Application Testing.png

Compare high-purity HPMC and industrial-grade HPMC for construction and daily-chemical formulations. Learn when impurities affect clarity, hydration, and consistency, why viscosity and substitution matter, and how to select a suitable grade through controlled testing and supplier documentation.

12 October 2026
HEC And HEMC Liquid Fertilizer Comparison.jpg

Compare HEC vs HEMC in liquid fertilizers and learn how each cellulose ether affects micronutrient compatibility, viscosity, suspension stability, pH control, chelated trace elements, and fertigation performance. Find practical testing steps for stable fertilizer formulations.

26 September 2026
Cellulose Ether Performance Testing.jpg

This article compares HPMC and HEMC for surface tension reduction and wetting performance in construction and daily chemical applications. It explains the chemical differences between Hydroxypropyl Methyl Cellulose and Hydroxyethyl Methyl Cellulose, evaluates their effects on spreading, viscosity, water retention, workability, and adhesion, and provides practical guidance for selecting the right cellulose ether grade for tile adhesive, wall putty, cement render, skim coat, gypsum plaster, coatings, and personal-care formulations.

28 September 2026
HPMC Applications In Construction.jpg

Discover how construction-grade HPMC improves tile adhesive, cement mortar, wall putty, gypsum plaster, EIFS, and self-leveling compounds. Learn HPMC water-retention mechanisms, selection factors, testing practices, and formulation insights from a professional cellulose ether manufacturer.

29 September 2026

Telephone

+86-131-7602-7703
​Copyright © Shandong Shengda New Material Co., Ltd. All Rights Reserved.

Products

Solution

Support

About

Contact Us for Your Needs

Our main products include HPMC, HEMC and HEC.