Ra'ayoyi: 243 Mawallafi: Shengda Lokacin Bugawa: 2026-08-31 Asalin: Shafin
Menu na abun ciki
>> Babban Ayyuka na HPMC a Dry-Mix Mortar
● Yadda HPMC ke Inganta Aikin Turmi Siminti
>> Riƙewar Ruwa don ƙarin Sarrafa Magani
>> Rheology da Kwarewar Mai Shigarwa
>> Adhesion Sakamakon Matsayin Tsari ne
>> HPMC na yumbu Tile Adhesive
>> HPMC don Wall Putty da Skim Coat
>> HPMC da HEMC na Cement Render da Plaster
>> HPMC na Gypsum Plaster da Haɗin Haɗin gwiwa
>> HPMC don Turmi Mai hana ruwa Siminti
● HPMC, HEMC da HEC: Zaɓin Madaidaicin Cellulose Ether
>> Abubuwan Da Ke Tasirin Zaɓin Grade na HPMC
● Hanya Mai Kyau don Auna HPMC a Tsarin Turmi
>> Mataki 1: Ƙayyade Samfurin da Ya Ƙare
>> Mataki 2: Gano Manufofin Ayyuka
>> Mataki na 3: Kwatanta Fiye da Daraja ɗaya
>> Mataki 4: Haɓaka sashi a hankali
>> Mataki na 5: Tabbatar da Ƙarƙashin Sharuɗɗa na Gaskiya
● Matsalolin Samuwar HPMC na gama gari da Magani
● Me yasa Taimakon Ƙirar Ƙirƙirar Ƙirƙirar Sakamako Mai Kyau
● Gina Dogaran Dry-Mix Mortar Performance Tare da Shengda
>> Menene HPMC ke yi a cikin tile adhesive?
>> Menene bambanci tsakanin HPMC da HEMC?
>> Nawa ya kamata a yi amfani da HPMC a turmi?
>> Yawancin HPMC na iya shafar ƙarfin turmi?
>> Shin HPMC ta inganta riƙe ruwa a turmi siminti?
>> Shin HPMC za ta iya maye gurbin foda polymer da za a iya tarwatsawa a cikin mannen tayal?
>> Shin HPMC ya dace da aikace-aikacen gini na yanayin zafi?
● Magana
Hydroxypropyl Methyl Cellulose ( HPMC ) shine maɓalli na aiki mai mahimmanci a cikin kayan gini na bushe-bushe na zamani. A cikin tile adhesives, siminti renders, bango putties, gypsum plasters da waterproofing turmi, da hakkin cellulose ether taimaka masana'antun cimma mafi alhẽri ruwa riƙewa, aiki aiki, bude lokaci, adhesion da anti-sag yi..
Ga masu kera turmi mai bushe-bushe, HPMC ba kawai foda ce mai kauri ba. Yana rinjayar yadda samfurin ke watsewa a cikin ruwa, yana haɗuwa a cikin masana'anta, yaduwa a bango, yana riƙe da danshi akan abin da ke sha kuma yana haɓaka aikin sa na ƙarshe bayan warkewa.
Shandong Shengda New Material Co., Ltd. yana haɓakawa da kera HPMC, Hydroxyethyl Methyl Cellulose ( HEMC ) da Hydroxyethyl Cellulose ( HEC ) ga abokan ciniki da ke neman daidaito, takamaiman aikace-aikacen cellulose ether mafita.
HPMC shine ether cellulose maras ionic wanda aka samo daga cellulose, polymer na halitta. Lokacin da aka haɗe shi da ruwa, HPMC yana yin ruwa kuma yana haifar da tsarin rheological mai sarrafawa a cikin siminti ko kayan tushen gypsum.
Wannan tsarin yana taimakawa sarrafa motsin ruwa, inganta haɗin turmi da kuma samar da daidaiton aikace-aikacen da ya fi dacewa.
A aikace, HPMC-jin gini na iya taimaka wa masana'antun turmi su ƙirƙira samfuran da ke da sauƙin haɗawa, mafi sauƙi don amfani kuma mafi aminci a ƙarƙashin yanayin wuraren aiki daban-daban.

HPMC na iya tallafawa maƙasudin ayyuka da yawa:
- Riƙewar ruwa don rage asarar danshi da wuri
- Ƙarfin aiki don haɗawa mai santsi da trowelling
- Buɗe lokaci don ƙarin sassaucin shigarwa
- Ayyukan anti-sag don aikace-aikacen tsaye
- Haɗin kai don ingantaccen turmi jiki da daidaito
- Taimakon mannewa ta hanyar mafi kyawun tuntuɓar ƙasa da magani mai sarrafawa
- Ingancin saman don mafi santsin ƙarewa a cikin putty, skim gashi da filasta
Ayyukan ƙarshe ya dogara da cikakken tsari. Nau'in siminti, tsarin filler, foda polymer foda, sitaci ether, buƙatar ruwa, hanyar haɗuwa da yanayin muhalli duk suna tasiri sakamakon.
HPMC yana haɓaka aikin turmi ta hanyar daidaita riƙon ruwa da sabbin maganganu na yanayi. Waɗannan ayyuka guda biyu suna da alaƙa sosai.
Lokacin da turmi ya yi asarar ruwa da sauri, yana iya zama da wahala yaduwa, bushewa ba daidai ba ko kuma kasa gina isasshiyar tuntuɓar ƙasa. Wannan ya zama ruwan dare musamman akan mason ƙorafi, tubalan kankare mai iska, busasshiyar saman kankare da wuraren aikin yanayi mai zafi.
Siminti yana buƙatar ruwa don yin ruwa yadda ya kamata. Idan ruwa ya ɓace da sauri bayan aikace-aikacen, turmi na iya rasa ƙarfin aiki kuma maiyuwa ba zai haɓaka abubuwan haɗin kai ko ƙarewa ba.
HPMC yana taimakawa rage gudun hijirar ruwa a cikin rigar turmi. Wannan yana ba kayan ƙarin lokaci don kasancewa mai iya aiki kuma yana taimakawa kula da danshi yayin farkon matakin warkewa.
Ga masana'antun, mafi kyawun riƙe ruwa na iya ba da gudummawa ga:
- Ƙarin kwanciyar hankali bayan haɗuwa
- Mafi kyawun aikace-aikacen akan manyan abubuwan sha
- Rage bushewa da sauri yayin yanayin zafi ko iska
- Tsawon lokacin aiki don masu sakawa
- Ƙarin ci gaban ƙasa mai uniform
- Ingantattun yanayi don shayarwar siminti
Rheology ya bayyana yadda turmi ke gudana, yadawa, tsayayya da motsi da farfadowa bayan an gauraye shi ko aka murƙushe shi. Yana tasiri sosai yadda mai sakawa ke sanin samfurin.
Madaidaicin ma'auni na HPMC na iya taimakawa turmi ya tsaya tsayin daka akan tudu da saman tsaye yayin da har yanzu yana yaduwa cikin matsin lamba.
Misali, mannen tayal ya kamata ya samar da tsattsauran ramuka mai tsafta. Kada ya ji dauri da yawa, ruwa ko wahalar tsefewa. Gilashin bango ya kamata ya yi yawo a hankali a saman saman ba tare da ja, yaga ko bushewa da sauri ba.
Manufar ba shine matsakaicin kauri ba. Manufar madaidaicin bayanin martabar aikace-aikacen da ke da sauƙin amfani da maimaituwa a cikin batches samarwa.
HPMC tana goyan bayan yanayin da ake buƙata don mannewa mai ƙarfi, amma mannewa baya dogara akan ether cellulose kaɗai.
Amintaccen tsarin turmi yana buƙatar daidaitattun ma'auni na:
- Siminti da nau'in ɗaure
- Gyaran polymer
- Girman daraja
- Zaɓin filler ma'adinai
- Ruwa-da-foda rabo
- Cellulose ether sa da sashi
- Substrate shiri
- Kauri aikace-aikace
- Yanayin zafi da yanayin warkewa
Don haka, zaɓin HPMC ya kamata koyaushe ya kasance ingantacce a cikin dabarar kasuwanci ta ƙarshe maimakon kimantawa ta hanyar bayanan danko kawai.
Tile m na ɗaya daga cikin buƙatun busassun aikace-aikacen gauraya. Dole ne ya kasance mai iya aiki bayan haɗawa, yaɗa sumul a ƙarƙashin tulun da aka sani, riƙe fale-falen fale-falen a wuri da kiyaye isassun mannewa yayin aikin shigarwa.
HPMC yana taimakawa masana'antun tayal don haɓakawa:
- Cakuda santsi
- Riƙewar ruwa
- Rashin ƙarfi
- Ma'anar Ridge
- Lokacin budewa
- Tile daidaitacce
- Halin hana zamewa a tsaye
- Substrate wetting da lamba kwanciyar hankali
Don aikace-aikacen bangon tsaye, ƙirar dole ne ta samar da isasshen jiki don sarrafa motsin tayal ba tare da wahala ba a yadawa. Don manyan fale-falen fale-falen fale-falen fale-falen buraka, buɗaɗɗen lokaci da yanayin haɗin kai suna da mahimmanci musamman saboda masu sakawa galibi suna buƙatar tsawon lokacin daidaitawa da madaidaiciyar canja wurin mannewa.
Ƙararren mannen tayal ɗin da aka ƙera yakan haɗa ether cellulose tare da siminti, yashi mai daraja, ma'adinan ma'adinai da masu gyara polymer. Kowane bangare yana rinjayar aikin ƙarshe.
Fuskar bangon bango da rigar skim na buƙatar santsi, mai tsami da daidaiton jin daɗin aikace-aikacen. Kayan ya kamata ya cika ƙananan lahani, yada a ko'ina, ya kasance mai aiki a lokacin kammalawa da kuma samar da wuri mai dacewa don yashi da zane.
HPMC na iya taimakawa ingantawa:
- Yaduwa mai laushi
- Riƙewar ruwa
- Ingantaccen ɗaukar hoto
- Daidaitawar saman
- Adhesion zuwa substrate
- Rage alamun ja
- Inganta lokacin sake aiki
- Yanayin sarrafa fashe yayin bushewa
Kalubalen ƙira na gama gari shine daidaita riƙe ruwa tare da aikin yashi da saurin bushewa. Yin kauri mai yawa zai iya sa kayan suyi nauyi ko m, yayin da rashin isasshen ruwa zai iya haifar da bushewa da sauri da rashin jin daɗin aikace-aikacen.
Batun siminti, turmi na masonry da romin filasta dole ne su kasance masu karko yayin hadawa, aikace-aikace da magani. Dole ne samfurin ya riƙe siffarsa a saman saman tsaye yayin da ya kasance mai sauƙin yadawa da matakin.
Ana amfani da HPMC da HEMC don ingantawa:
- Turmi daidaito
- Riƙewar ruwa
- kwanciyar hankali a tsaye
- Halayyar tashin hankali
- Pumpability
- Ƙarshen saman
- Tsage juriya
- Sharuɗɗan haɗin gwiwa
Ana iya zaɓar HEMC lokacin da tsari ya buƙaci ma'auni daban-daban na rheology, halayen aiki ko amsawar zafin jiki. Mafi kyawun zaɓi ya dogara da tsarin ɗaure da hanyar aikace-aikacen da ake so.
Abubuwan da ke tushen gypsum suna da halayen aiki daban-daban daga turmi siminti. Suna buƙatar amfani da ruwa mai sarrafawa, aikace-aikacen santsi, halayen saiti mai tsinkaya da ƙare mai inganci.
HPMC-jin gini na iya tallafawa filastar gypsum da fili ta haɗin gwiwa ta haɓaka:
- Cakuda uniformity
- Yadawa
- Slip da aikace-aikace jin
- Riƙewar ruwa
- Santsin saman
- Yanayin mannewa
- Kula da lokacin aiki
Matsayin da aka zaɓa ya kamata ya kasance mai jituwa tare da masu ɗaukar nauyi, masu kara kuzari, masu filaye da sauran abubuwan da ake ƙara gypsum. Ƙaramin daidaitawa a cikin adadin ether cellulose na iya tasiri sosai ga yanayin saiti da jin aikace-aikacen.
Rubutun hana ruwa na siminti da turmi suna buƙatar daidaiton daidaito, amintaccen lamba da yanayin aikace-aikacen sarrafawa. Dangane da dabarar, HPMC na iya goyan bayan buroshi, tawul ko aikace-aikacen feshi.
Babban fa'idodin na iya haɗawa da:
- Better hadawa daidaito
- Inganta ruwa
- Aikace-aikace mai laushi
- Ingantaccen haɗin kai akan saman saman tsaye
- Ingarin samuwar rigar-fim mai tsayayye
- Inganta jin daɗin aiki
Dole ne koyaushe a kimanta aikin hana ruwa ta amfani da cikakken tsari. Siminti siminti, zaɓin polymer, tsarin filler da kowane nau'in hydrophobic ko abubuwan haɓakawa sun kasance mahimman abubuwa.
HPMC, HEMC da HEC duk cellulose ethers ne, amma ba su canzawa a kowace dabara. Dacewar su ya dogara da aikace-aikacen, albarkatun ƙasa, yanayin zafi da aikin manufa.
| Babban | Matsayin Gine-gine Na Musamman | Babban Abubuwan La'akari |
|---|---|---|
| HPMC | Fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen) da bangon bango, mai sanyawa, rigar skim, filastar gypsum | Riƙewar ruwa, iya aiki, buɗaɗɗen lokaci, halayen anti-sag |
| HEMC | Tile m, siminti ma'auni, na musamman turmi | Ma'auni na Rheology, iya aiki, amsawar zafi |
| HEC | Wasu tsarin gine-gine da rufin ruwa | Kauri, kwanciyar hankali da daidaituwa a cikin tsarin tushen ruwa |
Zaɓin daidai yakamata ya fara da sakamakon aikace-aikacen da ake buƙata maimakon ma'aunin fasaha guda ɗaya.
| Factor Factor | Me Yasa Yayi Muhimmanci |
|---|---|
| Dankowar jiki | Yana tasiri mai kauri, haɗin kai da riƙe ruwa |
| Girman barbashi | Yana shafar watsawa da saurin ruwa |
| Riƙewar ruwa | Yana rinjayar lokacin aiki da yanayin warkewa |
| Gel zafin jiki | Mahimmanci ga aikace-aikacen dumi-yanayin yanayi |
| Shigar da iska | Zai iya rinjayar yawa, ƙarfi da ƙarewar ƙasa |
| Daidaituwa | Yana ƙayyade hulɗa tare da siminti, polymers da ƙari |
| Hanyar aikace-aikace | Yana tasiri rheology bukatun don hannu, fesa ko aikace-aikacen famfo |
| Yanayi | Zafi, iska da zafi suna shafar asarar danshi da lokacin aiki |
Samfurin danko mai girma ba shine mafi kyawun zaɓi ta atomatik ba. A wasu dabaru, ƙaramin darajar danko a ingantaccen sashi na iya samar da ingantaccen aiki, ƙarancin buƙatar ruwa da ingantaccen samarwa.
Zaɓin ether cellulose ya kamata a dogara ne akan gwaji maimakon zato. Tsarin kimantawa na yau da kullun yana taimaka wa masana'anta rage zagayowar sake fasalin da inganta daidaito.
Fara da bayyana aikace-aikacen a sarari:
- yumbu tile m
- Wall putty
- Skim gashi
- Ciminti
- Masonry turmi
- Gypsum plaster
- Haɗin haɗin gwiwa
- Turmi mai hana ruwa siminti
Kowane samfurin yana da buƙatu daban-daban don daidaito, buɗe lokaci, haɗin gwiwa, halayen anti-sag da saitin bayanin martaba.
Ƙirƙiri jerin maƙasudai da za a iya aunawa kafin zaɓin darajar HPMC. Abubuwan gwaji na yau da kullun sun haɗa da:
- Riƙewar ruwa
- Lokacin hadawa
- Turmi daidaito
- Lokacin budewa
- Zamewar tsaye
- mannewa mai ƙarfi
- Saita lokaci
- Yawan yawa
- Abubuwan da ke cikin iska
- Ƙarfin matsi
- Siffar saman
- Aikace-aikacen jin
Gwada makin HPMC ko HEMC da yawa a ƙarƙashin sharuɗɗan ƙira iri ɗaya. Yi amfani da kwatancen sashi mai sarrafawa domin sakamakon yana da ma'ana.
Kyakkyawan shirin gwaji yakamata ya kwatanta:
- daidaito na farko
- daidaito bayan tsayawa
- Riƙewar ruwa
- Halayen aikace-aikacen
- bonding hali
- Saitin halaye
- Ƙarfafa haɓaka
Kada ku ɗauka cewa mafi girman sashi koyaushe zai samar da mafi kyawun aiki. Matsakaicin ether na cellulose zai iya haifar da manne maras so, buƙatar ruwa mai yawa, ƙarin shigar iska ko saitin hankali.
Madaidaicin sashi shine matakin da ke ba da sakamakon aikace-aikacen da ake buƙata yayin kiyaye ƙarfi, kwanciyar hankali da ƙimar farashi.
Gwajin dakin gwaje-gwaje yana da mahimmanci, amma yanayi-kamar filin suna da mahimmanci daidai. Gwada dabarar ƙarƙashin yanayin da ake tsammani na zafin jiki, zafi, ɗaukar ƙasa da kayan haɗawa.
Manne tayal da ke aiki da kyau a cikin dakin gwaje-gwaje mai sarrafawa na iya yin yanayi daban-daban akan bango mai zafi, busasshiyar ko a cikin yanayin samarwa mai sauri.
| Batu na gama gari | Mai yuwuwar Dalili | da aka ba da shawarar Jagora |
|---|---|---|
| Turmi yana jin m sosai | Dankowar HPMC ko sashi ya yi yawa | Gwada ƙarancin danko ko rage sashi |
| Riƙewar ruwa bai isa ba | Ayyukan ether na Cellulose yayi ƙasa sosai | Ƙimar mafi girman matakin riƙe ruwa |
| Tile m sags a bango | Ma'aunin Rheology bai isa ba | Bitar HPMC, sitaci ether da tsarin filler |
| Lokacin buɗewa ya yi gajere sosai | Rashin ruwa da sauri ko kuma rashin dacewa | Inganta riƙon ruwa da tantance sha substrate |
| Turmi yana haɗuwa a hankali | Halin watsawa bai dace ba | Yi kimanta girman barbashi da tsarin hadawa |
| Ƙarfin yana ƙasa da yadda ake tsammani | Yawan iska, yawan buƙatar ruwa ko yawan adadin kuzari | Haɓaka sashi da bincika yawa da abun cikin iska |
| An jinkirta saitin | Yin hulɗa tare da siminti ko ƙari | Yi bitar zaɓin sa da dacewa |
| Putty yana bushewa da sauri | Rashin ruwa yana da sauri sosai | Inganta riƙon ruwa da duba yanayin muhalli |
| Ƙarshen saman bai yi daidai ba | Formula ba ta da ma'auni | Bita makin filler, buƙatar ruwa da matakin ether cellulose |
Zaɓin ether cellulose ya fi tasiri lokacin da mai sayarwa ya fahimci samfurin da aka gama, kayan albarkatun gida da ainihin yanayin aikace-aikacen.
Tattaunawar fasaha mai amfani yakamata ta ƙunshi:
- Nau'in samfurin bushe-bushe da ake haɓaka
- Ƙirƙira na yanzu da tsarin danyen kayan aiki
- Kasuwar manufa da yanayin yanayi
- Substrate irin
- Kayan aikin samarwa
- Hanyar aikace-aikace
- Babban damuwa damuwa
- Matsayin fasaha ko tsammanin abokin ciniki
Wannan bayanin yana goyan bayan ingantaccen zaɓi na ƙira da haɓaka ƙira da sauri.
HPMC, HEMC da HEC suna taimakawa masana'antun busassun turmi don ƙirƙirar samfura tare da ingantaccen riƙon ruwa, iya aiki, buɗe lokaci da aikin aikace-aikace.
Sakamakon mafi ƙarfi ya fito ne daga daidaita ma'aunin ether cellulose zuwa ainihin aikace-aikacen, sannan inganta shi ta hanyar gwajin ƙira. Ko makasudin ya kasance mai santsi mai santsi na bango, mannen tayal mai tsayi mai tsayi, ingantaccen siminti ko filastar gypsum mai aiki, daidaitaccen ma'auni na ether cellulose da ƙirar ƙira.
Shandong Shengda New Material Co., Ltd. yana ba da mafita na ether cellulose ga masana'antun duniya na fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen fale-falen buraka, siminti, filastar gypsum, turmi mai hana ruwa da samfuran gini masu alaƙa. Ƙungiyarmu na fasaha za ta iya tallafawa zaɓin kayan aiki da gwajin aikace-aikacen dangane da buƙatun samfurin ku.
HPMC shine ether cellulose mai aiki wanda ke taka muhimmiyar rawa a cikin bushe-bushe kayan gini. Ƙarfinsa don inganta riƙewar ruwa, iya aiki, lokacin buɗewa da haɗin kai yana sa ya zama mai daraja don manne tayal, bangon bango, yin siminti, plaster gypsum da turmi mai hana ruwa.
Mafi kyawun sakamako ya dogara da fiye da zaɓin samfur mai cike da danko. Ya kamata masana'antun su kimanta HPMC, HEMC ko HEC bisa ga buƙatun samfuran da aka gama, tsarin albarkatun ƙasa, hanyar aikace-aikacen da yanayin muhalli na gida. Gwaji na yau da kullun da haɓaka ƙirar ƙira sun kasance masu mahimmanci don ingantaccen aikin kasuwanci.
HPMC yana taimakawa haɓaka riƙon ruwa, iya aiki, buɗe lokaci da trowelability a cikin mannen tayal na tushen siminti. Hakanan yana goyan bayan madaidaicin mannewa lamba da mafi kyawun halayen sag idan aka yi amfani da su cikin madaidaicin dabara.
HPMC da HEMC duka ethers ba na ionic cellulose ne da ake amfani da su a cikin kayan gini. Tsarin sinadaran su ya bambanta, wanda zai iya rinjayar rheology, riƙewar ruwa, yanayin aiki da amsa yanayin zafi. Mafi kyawun zaɓi ya dogara da dabarar manufa da yanayin aikace-aikacen.
Babu wani sashi guda daya dace da kowane turmi. Matsayin da ake buƙata ya dogara da matakin HPMC, nau'in siminti, tsarin filler, abun ciki na polymer, buƙatar ruwa, yanayin yanayi da aikin da ake so. Gwajin dakin gwaje-gwaje ya zama dole don gano adadin da ya dace.
Ee. Matsanancin HPMC na iya ƙara buƙatar ruwa, gabatar da ƙarin iska ko tasiri yanayin saiti. Waɗannan canje-canje na iya shafar yawa, ƙarfin haɗin gwiwa da ƙarfin matsawa. Ya kamata a inganta sashi don cikakken tsari.
Ee. HPMC yana taimakawa riƙe ruwa a cikin sabon turmi ta hanyar canza motsin ruwa a cikin kayan. Wannan na iya inganta iya aiki, rage bushewa da wuri da goyan bayan ƙarin sarrafa ruwan siminti.
A'a. HPMC da redispersible polymer foda hidima daban-daban ayyuka. HPMC galibi yana sarrafa riƙewar ruwa da rheology, yayin da ake amfani da foda na polymer gabaɗaya don haɓaka mannewa, sassauci da karko. Yawancin dabarar manne tayal suna amfani da kayan biyu.
HPMC na iya taimakawa rage saurin asarar danshi da inganta lokacin aiki a yanayin zafi ko bushewa. Koyaya, yakamata a gwada cikakkiyar dabarar a ƙarƙashin yanayin aikace-aikacen da ake tsammanin saboda zafin jiki, iska, zafi da shayar ƙasa duk suna shafar aiki.
1. LANDU. [Fahimtar HPMC: Aikace-aikace da Amfanin Gina ].
2. Chen, N., et al. [Injin Riƙe Ruwa na HPMC a Turmi Siminti ]. *Materials*, 2020.
3. Glinicki, MA, et al. [Tasirin Nau'in Siminti akan Abubuwan Rubutun Rubutun da aka gyara tare da Cellulose Ether Admixture ]. *Materials*, 2021.
4. Zhang, da dai sauransu. [Abubuwan Calcium Sulfoaluminate Turmi Siminti Wanda Hydroxyethyl Methyl Celluloses Ya Gyara Tare da Matsaloli daban-daban na Sauyawa ]. *Materials*, 2021.
5. ZKG International. [Buɗe Lokacin Buɗe - Bukatar Daidaita Mahimmin Siga ].
6. iTeh Standards Store. [TS EN 12004-1: 2017-Adhesives don fale-falen yumbu