● Me yasa Gel ɗin wanke wanke yana da wahala a ƙirƙira
● Menene Detergent Grade HEMC?
>> Mabuɗin Ayyuka na HEMC a cikin Wanki
>> Yadda Carbomer ke Gina Gel danko
● Detergent Grade HEMC vs Carbomer: Babban Bambance-bambance
● Me yasa Ethers Cellulose ke samun ƙasa a cikin Gel mai haske
>> Faɗin Daidaitawa Tare da Tsarin Surfactant
>> Rage Dogara akan Neutralization
>> Dandali na Sirri na Tushen Cellulose
● Tsallake Yana nufin Fiye da Bayyanawa
● Lokacin Zaba Detergent Grade HEMC
● Hanya Mai Kyau don Nuna HEMC da Carbomer
>> Tsarin Nuna Ƙirƙirar Ƙirƙiri Nasiha
● Ƙwararrun Ƙwararru: Yi la'akari da Dabarun Rheology Hybrid
● Gina Mafi kyawun Abubuwan wanke Gel tare da Shengda
>> Shin matakin HEMC na wanka ya dace da tsabtace ruwan wanka?
>> Shin HEMC yana buƙatar neutralization kamar carbomer?
>> Wanne ne ke samar da mafi kyawun gel: HEMC ko carbomer?
>> Shin HEMC ya fi ƙarfin gishiri fiye da carbomer?
>> Za a iya amfani da HEMC a wanke hannu da ruwan wanke-wanke?
>> Shin HEMC zai iya maye gurbin carbomer cikakke?
>> Menene yakamata a gwada kafin zabar kauri?
● Nassoshi
A m abin wanke-wanke gel tsarin abubuwa ne da yawa. Yana iya ƙunsar anionic, amphoteric, nonionic, ko cationic surfactants. Hakanan yana iya haɗawa da gishiri, ƙamshi, abubuwan kiyayewa, rinannun rini, abubuwan lalata, kaushi, sinadaran kashe ƙwayoyin cuta, da ƙari na aiki.
Kowane sashi na iya shafar tsabta, danko, kumfa, da kwanciyar hankali na dogon lokaci.
Babban kalubalen shine ƙirƙirar ma'auni daidai. Mai kauri dole ne ya gina danko ba tare da sanya tsarin ya zama m, kitse, rashin kwanciyar hankali, wahalar kerawa, ko rashin jin daɗi don amfani ba.
Nasarar ingantaccen tsarin gel ɗin yana buƙatar:
- High tsabta don m shiryayye gabatarwa
- Stable danko a lokacin samarwa da ajiya
- Sauƙaƙan zubewa ko yin famfo daga fakitin da aka zaɓa
- Halin ɓarna mai ƙarfi don ingantaccen amfani mai amfani
- Gishiri da daidaituwar surfactant
- Tsayayyen aikin pH
- Daidaita kamshi da rini
- Amintaccen tsari-zuwa-tsari
- Ayyukan aiki a ma'aunin samarwa
Tsarin da ya bayyana a sarari nan da nan bayan haɗuwa na iya gazawa daga baya. Danko na iya sauke bayan daidaitawar gishiri. Turare na iya haifar da hazo. Ƙananan yanayin zafi na iya canza halin kwarara. Kumfa na iska na iya shafar bayyanar gani bayan cikawa.
Abin da ya sa ya kamata zaɓin kauri ya dogara da cikakken tsari maimakon gwaji mai sauƙi na tushen ruwa.
Detergent daraja HEMC ne mai narkewar ruwa, nonionic cellulose ether. Ana samar da shi daga cellulose ta hanyar gyaran gyare-gyaren sinadarai tare da hydroxyethyl da methyl kungiyoyin.
Wannan tsarin yana ba HEMC haɗin mai amfani mai narkewa na ruwa, aiki mai kauri, sarrafa rheology, da dacewa a yawancin tsarin ruwa.
A cikin na'urorin wanke-wanke da tsaftacewa na sirri, HEMC na iya taimakawa ƙirƙirar jiki, sarrafa kwarara, haɓaka kwanciyar hankali, da goyan bayan samfurin samfur mai ban sha'awa.
Detergent matakin HEMC na iya samar da:
- Ci gaban danko a cikin samfuran tsaftacewa na tushen ruwa
- Santsi da halin kwarara mai sarrafawa
- Rheology mai ƙarfi mai ƙarfi don sauƙin zubawa da rarrabawa
- Dace da yawa surfactant tsarin
- Riƙewar ruwa da daidaita tsarin tsari
- Ingantacciyar kulawa yayin samarwa
- Wani zaɓi na tushen cellulose
- Taimako don bayyanannun samfurin ko bayyananne
Saboda HEMC ne nonionic, ba ya dogara da wani tsari na ionization don gina danko kamar yadda carbomer. Wannan na iya sa ya zama abin ban sha'awa ga wasu tsarin arziƙin surfactant.
Koyaya, aikin HEMC har yanzu yana dogara da ƙimar da aka zaɓa, sashi, yanayin hydration, tsarin hadawa, matakin electrolyte, pH na ƙarshe, rabon surfactant, da zafin jiki.
Carbomer shine polymer acrylic acid mai haɗe-haɗe da aka yi amfani da shi azaman mai kauri, wakili na gelling, taimakon dakatarwa, da mai gyara rheology.
Ana amfani dashi sosai a cikin gels na kwaskwarima, masu tsabtace hannu, samfuran kula da fata, samfuran tsabtace mutum, da aikace-aikacen kula da gida da aka zaɓa.
Carbomer sananne ne don samar da gels masu haske sosai tare da danko mai ƙarfi a ƙananan matakan ƙari.
Carbomer yawanci yana buƙatar matakai masu mahimmanci guda uku:
1. Watsewa
Dole ne a tarwatsa foda a hankali a cikin ruwa don rage girman agglomerates.
2. Ruwan ruwa
Polymer yana buƙatar lokaci don jika da ruwa cikakke.
3. Neutralization
Ana ƙara neutralizer mai dacewa don haɓaka pH da kunna ci gaban danko.
Kafin neutralization, carbomer polymer sarƙoƙi suna da ɗan ƙaramin ƙarfi. Bayan neutralization, da polymer sarkar fadada. Wannan yana haifar da hanyar sadarwa mai girma uku wanda ke kama ruwa kuma yana gina danko gel.
Tsarin zai iya ba da sakamako mai ban sha'awa. Duk da haka yana iya zama mai kula da tsari na sinadarai, sarrafa pH, tattarawar electrolyte, zaɓin surfactant, da zaɓin tsaka tsaki.
| Ayyuka Factor Factor | Detergent Grade HEMC | Carbomer |
|---|---|---|
| Nau'in polymer | Nonionic cellulose ether | Acrylic acid polymer tare da crosslinked |
| Main thickening inji | Hydration da polymer-sarkar hulda | Polymer kumburi bayan neutralization |
| Bukatar neutralization | Yawancin lokaci ba babban matakin kunnawa danko bane | Yawanci ana buƙata don babban danko |
| Daidaita tsarin Surfactant | Sau da yawa m a gauraye surfactant tsarin | Ya dogara da ƙarfi akan zaɓaɓɓen sa da ƙirar ƙira |
| Sanin gishiri | Zai iya ba da haƙuri mai amfani dangane da ƙima da tsarin | Maki na al'ada na iya zama mai kula da electrolytes |
| Yiwuwar tsabta | Za a iya goyan bayan bayyanannun gels na translucent | Sau da yawa yana ba da gaskiya sosai |
| Bayanin Rheology | Santsi, mai amfani, kwarara mai juzu'i | Short, mai arziki, bayanin martaba mai kama da gel |
| Bukatun sarrafawa | Sarrafa watsawa da hydration | Watsawa, hydration, da madaidaicin tsaka tsaki |
| Matsayin sashi | Cellulose tushen da nonionic | Roba acrylic polymer |
| Aikace-aikace gama gari | Abubuwan wanke-wanke, wanke hannu, sabulun wanka, masu tsaftace gida | Gel mai tsabta, gels kulawa na sirri, zaɓaɓɓen samfuran kulawa na gida |
Darasi mafi mahimmanci shine mai sauƙi: babban nuna gaskiya kadai bai isa ba.
Gel mai bayyananniyar gani na iya zama mara ƙarfi bayan ƙara ƙamshi, hawan zafin jiki, daidaitawar gishiri, ko adana dogon lokaci. Mafi kyawun mai kauri shine wanda ke ba da ingantaccen aiki a duk tsarin da aka gama.
Cellulose ethers suna samun ƙarin kulawa saboda abubuwan da aka tsara suna canzawa.
Masu masana'anta suna buƙatar fayyace maɓuɓɓugan ruwa waɗanda ke yin aiki da dogaro a cikin ƙarin hadaddun tsarin surfactant. Har ila yau, suna son aiki mai ƙarfi, daidaitawar sinadarai masu sassauƙa, haɓakar sikelin da ake iya faɗi, da ƙarin zaɓuɓɓuka don haɓaka samfurin tushen cellulose.
Abubuwan wanke ruwa na zamani sukan yi amfani da surfactant fiye da ɗaya.
Tsarin tsari na yau da kullun na iya haɗawa da:
- Anionic surfactants don aikin tsaftacewa
- Amphoteric surfactants don kumfa da laushi
- Nonionic surfactants don cire mai
- Solubilizers don kwanciyar hankali na kamshi
- Gishiri don daidaita danko
- Abubuwan kiyayewa da masu lalata don kariyar samfur
Mai kauri mara nauyi kamar HEMC na iya zama da amfani saboda gabaɗaya yana gabatar da ƙarancin hulɗar da ke da alaƙa da caji cikin tsarin.
Wannan baya nufin kowane maki HEMC ya dace da kowane abu don wanke wanke. Matsakaicin matakan lantarki, fakitin surfactant m, babban abubuwan aiki, da wasu kaushi na iya shafar aikin sa.
Har yanzu, matakin wanke-wanke HEMC yana ba da ƙaƙƙarfan mafari ga masu ƙira suna gina madaidaitan gels masu arziƙi.
Tsarin Carbomer na iya buƙatar neutralization a hankali. Ƙananan canji a cikin pH, nau'in neutralizer, ko jerin kari na iya rinjayar danko, tsabta, da rubutun gel na ƙarshe.
HEMC baya dogara da neutralization a matsayin babban abin da ke haifar da ci gaban danko.
Wannan na iya ba da fa'idodi masu amfani yayin tsarawa da samarwa:
- Kadan sauye-sauyen danko da ke tafiyar da pH
- Ƙarin hanyoyin masana'antu masu sassauƙa
- Ƙananan haɗari na yawan amfani da neutralizer
- Sauƙaƙan hanyoyin daidaita danko
- Ƙarin haɓakar danko kai tsaye yayin hydration
- Ma'auni mai sauƙi mai sauƙi daga dakin gwaje-gwaje zuwa masana'anta
Ƙarshen pH ya kasance mai mahimmanci don ingancin samfur, adanawa, aminci, zaɓin mabukaci, da dacewa tare da sauran sinadaran. Bambancin shine HEMC baya buƙatar daidaita pH don buɗe ainihin aikin kauri.
Cellulose yana daya daga cikin mafi yawan polymers na halitta a duniya. Ana ƙera ethers cellulose ta hanyar gyare-gyaren sarrafawa don cimma ruwa mai narkewa da aiki a cikin ƙirar masana'antu.
Don samfuran wanki, wannan na iya tallafawa tattaunawar haɓaka samfura a kusa da:
- Tsarin kauri na tushen Cellulose
- Asalin danyen kayan halitta da aka samo asali
- Zaɓin Nonionic polymer
- Madaidaitan labarun sinadarai
- Ƙarin bambance-bambancen zaɓuɓɓukan rheology-mai gyara
Yakamata a yi bitar da'awar da aka gama-samfurin koyaushe bisa ga ma'auni, hanyar samo asali, ƙa'idodin gida, buƙatun takaddun shaida, da samuwan shaida.
Gel mai tsabta ba kawai sakamakon gani ba. Sakamakon aiki ne.
Ya kamata masu ƙira su kimanta tsabta tare da danko, kwarara, kwanciyar hankali, dacewa da ƙamshi, halayen marufi, da juriya na zafin jiki.
| Yankin Ƙimar | Abin da za a tantance | Me ya sa yake da mahimmanci |
|---|---|---|
| Bayyanar gani | Haze, nuna gaskiya, kumfa, canjin launi | Yana goyan bayan bayyanar babban shiryayye |
| Dankowar jiki | Dankowar farko da tsufa | Yana nuna daidaiton ajiya |
| Rheology | Pourability, famfo, stringiness | Yana rinjayar kwarewar mabukaci |
| Haƙuri gishiri | Dankowa bayan ƙara electrolyte | Yana nuna ainihin yanayin wanki |
| Daidaitawar surfactant | Kwanciyar hankali bayan haɗuwa da surfactant | Yana rage haɗarin ƙira |
| Daidaituwar kamshi | Tsallakewa bayan ƙara ƙamshi | Yana hana hazo da rabuwa |
| Yanayin zafi kwanciyar hankali | Ayyukan bayan ajiya mai zafi da sanyi | Yana goyan bayan amincin jigilar kaya |
| Juriya-narke | Bayyanawa bayan hawan hawan zafin jiki | Yana rage haɗarin gazawar yanayi |
| Halin tattarawa | Rarraba daga famfo, iyakoki, da kwalabe | Yana kare gamsuwar mai amfani na ƙarshe |
Gel mai tsabta ba ta atomatik ba ce mai tsayayye.
Dole ne kayan wanka na kasuwanci ya kasance mai kyan gani da sauƙin amfani daga ranar farko ta samarwa har zuwa ƙarshe na mabukaci.
Matsayin wanke-wanke HEMC na iya zama zaɓin da ya dace lokacin da samfurin yana buƙatar ɗanɗano mai santsi, aiki mai dacewa, da dacewa tare da hadadden tushe na surfactant.
Yi la'akari da HEMC lokacin da:
- Tsarin ku ya ƙunshi gauraye surfactants
- Kuna son nonionic cellulose ether thickener
- Kuna buƙatar nau'in gel mai santsi, mai zubowa
- Kuna so ku rage dogaro akan neutralization
- Kuna haɓaka sabulun wanke hannu ko ruwa
- Kuna tsara ruwan wanke-wanke
- Kuna ƙirƙirar gels-tsaftar gida
- Kuna buƙatar kimanta aiki a cikin tsarin da ke ɗauke da gishiri
- Kuna son zaɓin kauri na tushen cellulose
- Kuna buƙatar kulawar rheology mai sassauƙa don nau'ikan fakiti daban-daban
HEMC na iya zama da amfani musamman inda samfur ke buƙatar danko ba tare da tsayayyen tsarin gel ba.
Misali, wanke hannu na iya buƙatar isasshen danko don bayyana ƙima a cikin kwalbar famfo. A lokaci guda kuma, dole ne ya bazu cikin sauƙi, ya shimfiɗa da kyau tsakanin hannaye, kurkura da tsabta, da kula da aikin kumfa.
Matsayin da aka zaɓa da kyau na HEMC na wanka zai iya taimakawa daidaita waɗannan buƙatun.
Carbomer na iya zama mafi kyawun zaɓi lokacin da babban makasudin shine babban tsabta da tsarin gel mai ƙarfi.
Yi la'akari da carbomer lokacin da:
- Babban burin ku shine babban bayyananne
- Tsarin ku na iya tallafawa karkatar da hankali
- Kuna buƙatar babban danko a ƙaramin matakin ƙarawa
- Kuna buƙatar wadataccen nau'in gel mai ɗan gajeren lokaci
- Ana iya sarrafa matakin electrolyte ɗin ku
- Kuna da ingantaccen tsarin kula da pH
- Ƙungiyar samar da ku ta saba da hydration na carbomer da neutralization
- Samfurin ku yana buƙatar tsarin gel mai yawan amfanin ƙasa
Carbomer na iya yin tasiri sosai a cikin madaidaicin gels masu tsabta. Koyaya, masu haɓakawa yakamata su zaɓi matakin a hankali saboda nau'ikan carbomer daban-daban na iya nuna halaye daban-daban a cikin tsarin mai ɗauke da gishiri ko surfactant-nauyi.
Ɗaya daga cikin kurakuran ƙira na yau da kullun shine gwada mai kauri kawai a cikin ruwan da ba shi da kyau.
Wannan na iya nuna ainihin iya yin kauri. Ba ya nuna ainihin aiki a cikin ƙirar da aka gama.
Hanyar da ta fi karfi ita ce a gwada darajar sabulun wanka HEMC da carbomer a cikin wani tushe mai mahimmanci da wuri-wuri.
1. Ƙayyade makasudin samfurin
Gano danko da ake buƙata, pH, tsabta, kumfa, matakin ƙamshi, nau'in fakiti, da yanayin ajiya.
2. Shirya tushe na zahiri na surfactant
Haɗa abubuwan da ake amfani da su, gishiri, abubuwan adanawa, abubuwan chelating, kaushi, da sauran mahimman kayan aikin.
3. Gwada allurai masu kauri da yawa
Ƙirƙiri madaidaicin amsa-sauri maimakon gwada maida hankali ɗaya kawai.
4. Sarrafa jerin hadawa
Yi rikodin saurin haɗuwa, zafin jiki, lokacin ruwa, ƙarin tsari, da yanayin daidaita pH.
5. Auna bayan cikakken ruwa
Kada ka dogara kawai ga karatun danko nan take. Bada isasshen lokaci don tsarin ya daidaita.
6. Ƙara ƙamshi da launi kafin kimantawa ta ƙarshe
Turare da rini na iya canza tsabta, solubility, da danko.
7. Gudun gwajin kwanciyar hankali
Gwada ma'ajin zafin jiki, ma'ajiyar zafin jiki mai girma, daskare-narke keke, da centrifugation idan ya dace.
8. Tabbatar da ma'aunin matukin jirgi
Kayan aikin samarwa na iya gabatar da yanayi daban-daban na juye, halayen hydration, da shigar iska.
A wasu hanyoyin, mafi kyawun sakamako baya zuwa ta amfani da kauri ɗaya kawai.
Tsarin rheology na matasan na iya haɗa ether cellulose tare da wani mai kauri mai jituwa don inganta kwarara, gina danko, daidaita ƙimar yawan amfanin ƙasa, ko goyan bayan dakatarwa.
Misali, HEMC na iya samar da jiki mai santsi da gudana mai amfani a cikin dabara mai wadatar surfactant. Mai gyara rheology na biyu zai iya tace tsarin gel ko inganta ɓangarorin dakatarwa.
Wannan tsarin zai iya haifar da ƙarin daidaiton aiki. Koyaya, yana buƙatar gwaji na horo.
Ƙara masu kauri da yawa ba tare da ƙayyadadden dalili ba na iya ƙara farashi, haifar da hazo, rikitarwa aiki, ko haifar da halayen rheological na ba zato ba tsammani.
Tambaya mafi kyau ba shine, 'Wane kauri ne ya fi karfi?'
Tambaya mafi fa'ida ita ce: Wanne tsarin kauri ne ke ba da tsayuwar da ake buƙata, danko, kwanciyar hankali sarrafa aiki, ƙwarewar mabukaci, da sarrafa farashi a cikin wannan madaidaicin dabarar wanki?
Shandong Shengda New Material Co., Ltd. yana mai da hankali kan bincike, haɓakawa, samarwa, da samar da samfuran HPMC, HEMC, HEC, da samfuran ether na cellulose masu alaƙa don abokan cinikin duniya.
Don masu kera wanki, masu ƙira, masu rarrabawa, da samfuran alamar masu zaman kansu, zaɓin mai kauri na iya shafar ingancin samfura da ingancin masana'anta. Madaidaicin ether cellulose na dama zai iya taimakawa wajen rage sake zagayowar sake fasalin, inganta daidaiton aiki, da ƙirƙirar samfurin gel mai tsabta tare da barga, rheology-friendly mabukaci.
Tuntuɓi Shandong Shengda New Material Co., Ltd. don tattauna samfurin HEMC na sabulu, jagorar fasaha, da mafitacin ether cellulose don ƙirar gel ɗin ku.

Ee. Za'a iya amfani da matakin da aka zaɓa da kyau na HEMC a cikin tsabtataccen wanka na ruwa, wankin hannu, ruwan wanke-wanke, da gels ɗin tsaftace gida. Tsaftar ƙarshe ta dogara da dabarar, gami da surfactants, gishiri, kamshi, sashi, yanayin sarrafawa, da kwanciyar hankali na ajiya.
A'a. HEMC gabaɗaya baya dogara ga neutralization a matsayin babban hanyar yin kauri. Carbomer yawanci yana buƙatar neutralization don faɗaɗa hanyar sadarwa ta polymer da ƙirƙirar babban danko gel.
Carbomer an zaɓi yadu don madaidaicin gels lokacin da aka inganta tsarin. HEMC kuma na iya goyan bayan fayyace ko fassarorin tsari. Sakamakon ƙarshe ya dogara da ƙayyadaddun tsari, gami da surfactants, electrolytes, turare, pH, da yanayin sarrafawa.
Ya dogara da darajar HEMC, nau'in carbomer, nau'in gishiri, maida gishiri, da tsarin surfactant. Makin carbomer na al'ada na iya zama mafi kula da electrolytes. Wasu ƙwararrun maki na carbomer an ƙirƙira su don ingantacciyar haƙurin electrolyte. Dukansu ya kamata a gwada su a cikin ginin da aka yi niyya.
Ee. Ana iya amfani da darajar HEMC don wanke hannu, sabulun ruwa, ruwan wanke-wanke, masu tsabtace gida, da sauran abubuwan da suka shafi ruwa wanda ke buƙatar sarrafa danko da ingantacciyar dabi'ar kwarara.
A wasu hanyoyin, i. HEMC na iya zama madadin da ya dace inda hali mara kyau, dacewa mai dacewa, kwarara mai santsi, da sauƙin sarrafawa sune fifiko. A cikin aikace-aikacen da ke buƙatar tsattsauran ra'ayi ko ƙaƙƙarfan tsarin gel mai samar da albarkatu, carbomer ko tsarin kauri na iya zama mafi dacewa.
Ƙimar tsabta, danko, rheology, kwanciyar hankali pH, haƙurin gishiri, daidaituwar surfactant, dacewa da kamshi, aikin kumfa, kwanciyar hankali zafin jiki, kwanciyar hankali-narke, da halayyar marufi. Hakanan ana ba da shawarar tabbatar da sikelin matukin jirgi kafin samarwa kasuwanci.
1. Ashland. [Natrosol™ Hydroxyethylcellulose don Gida, Masana'antu da Kula da Cibiyoyi ].
2. Ashland. [Kula da gashi: Natrosol™ Hydroxyethylcellulose ].
3. Lubrizol. [Carbopol® Polymer Excipients ].
4. Lubrizol. [Carbopol® Ultrez 20 Polymer ].
5. Lubrizol. [Carbopol® ETD 2020 Polymer .
6. Kimiyya Direct. [Abubuwan da ke shafar Halayen Rheological na Watsawar Carbomer a Matsakaicin Hydroalcoholic: Zuwa Haɓaka Tsarin Hannun Sanitizer Gel ].
7. Google Patents. [Gyaran Nonionic Cellulose Ethers, US4228277A .
8. Celotech. [Cellulose Ether don Kulawa na Gida da Mai Kauri ].